Polyester Spandex Air Covered Yarn

75d/36f + 20d White

75d/36f + 20d Black

75d/36f + 15d White

75d/36f + 15d Black

Naylon Spandex Air Covered Yarn

70d/24f + 20d White

70d/24f + 20d Black

70d/24f + 15d White

70d/24f + 15d Black

Spandex Air Covered  Yarn 

Naylon Air Covering Yarn 75d/24f+20

The strength and elongation of air covered yarn increases with the increase of the pre-draft ratio of spandex. When the draft reaches a certain value, the retraction of spandex yarn makes the outer fiber curl; with the increase of the predraft ratio, the percentage of spandex decreases.